bones206 said:
@Demented - good point about the water weight. Do we know if there was a drainage system installed prior to the collapse? It looked like white pvc drain pipe was hanging below the plaza slab in the parking garage tour video. But that may have been for something else.
The planter soil may have been quite saturated as well.
Ah, the planters. There's a chance those were full of water too, and I mean FULL.
3-4 years ago a contractor from the Miami area hired me to make some planters for a well known hotel down there. Wound up not doing the job, but his plans called for 2ftx2ftx10ft planters with no drainage, and mounting tabs so he could just lag bolt it down to the concrete where they wanted it internally.
I don't think a drainage system was installed prior to, or work had even begun on fixing the issue with the drainage. I'm an hour north of Surfside, and up here, from the 21st to the early hours of the 24th, we received 2.44" of rain, and it's been on the drier side here compared to more south. It's been mostly cloudy too, and water has just been sitting here in puddles. Especially areas where there's a lack of drainage, 3-8" of water easily pools up where allowed. Sloped drainage areas with clogged drains, especially around landscaping day or windy days when lawn debris is everywhere, are all too common.
Even though there is a pipe hanging, that may have absolutely nothing to do with the fire system. (Plus, if the penthouse collapsed first, where were those fire system alerts?)
The slab could have fully cracked through, or even epoxy injection repairs could have failed, allowing the sitting water on top to start to flow through cracks, which could explain what we are seeing. To me it looks like no more than a small amount of water being poured or drained, similar to the amount you'd see coming from a gutter/drain system, not a pressurized system for fire suppression. I've seen those break first hand, and you actually get gushing, not the slow, 80 year old man prostate dribble coming from the upper deck in the tiktok video.
Precision guess work based on information provided by those of questionable knowledge
Aerospace/Industrial/Medical/Structural
SoFla