Hi,
We need to carry out ultrasonic testing of welds on 106 mm thick SA 516 Gr. 70 Plate with 6mm thick SS 316 weld overlay. What would be the effect of attenuation and how it can be taken care during Ultrasonic tesing? Carrying out UT before overlay is not an option as UT need to be done after post weld heat treatment.
Please suggest recommended UT techniques for this case. Thanks in advance.
We need to carry out ultrasonic testing of welds on 106 mm thick SA 516 Gr. 70 Plate with 6mm thick SS 316 weld overlay. What would be the effect of attenuation and how it can be taken care during Ultrasonic tesing? Carrying out UT before overlay is not an option as UT need to be done after post weld heat treatment.