Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations dmapguru on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Quolifying thickness reducetion for forming head of pressure vessel in fabrication

Status
Not open for further replies.

mechengineer

Mechanical
Joined
Apr 19, 2001
Messages
268
Location
SG
Hi QC experts,
I have a vendor, the nominal dished head thickness is 14 mm, after forming 7 mm, the stress calculation thickness required is 6 mm. It is ok in deign/stress calculation. But I don't believe it is a good/qualified product with reduced a half of the nominal thickness after forming, some where thickness reduced from 14 mm to 7 mm. Any regulations from code, user's specifications and fabrication experience for qualifying the forming head thickness reduction?
Thanks
 
Depends on the required pressure. Someone needs to do a stress analysis using the actual thicknesses.
 
You don't give a lot of info, but I would check out UCS-79 (d)(2)(d)
 