Suspended operation, due to.... Out of subs 
The problem with sloppy work is that the supply FAR EXCEEDS the demand
The problem with sloppy work is that the supply FAR EXCEEDS the demand
Follow along with the video below to see how to install our site as a web app on your home screen.
Note: This feature may not be available in some browsers.
Dik said:sums it up, and you forgot to include that he fired anyone that didn't agree with him. 'De mortuis nil nisi bonum dicendum est' (don't speak ill of the dead) is not applicable... the guy was a POS and killed four others.
IRstuff said:FoS of 2.5 implies that you understand the material extremely well
There were plenty of people who *didn’t* disagree with him and happily pursued the venture with him. Plenty of people supplied to him, including it seems the main hull for the specific purpose of exploring at Titanic depth
Tug said:I wonder if the carbon fiber cylinder would be able to support itself without the titanium end caps?
Tomfh said:The thing worked 40 or so times, so wasn't a completely failed program. It's about the same failure rate as the space shuttle.
LittleInch said:It's just difficult to see how window failure is going to lead to implosion and complete disintegration of the the hull.
SwinnyGG said:But the hull was, in theory, designed for this depth and had some level of safety margin.
But the hull was, in theory, designed for this depth and had some level of safety margin.
So we just ignore the actual designers and builders of the hull do we?