HI
IS THERE ANY BODY CAN TELL ME WHAT IS THE P NOMBER AND GROUP NOMBER FOR A860 WPHY 65
REGARDS,
R.SALIMI
 
Replies continue below

Recommended for you

A860/A860M-00 is Standard Specification for Wrought High-Strength Low-Alloy Steel Butt-Welding Fittings, but there is no such ASME material existed as SA-860, so no P NOMBER AND GROUP NOMBER are available for this material.
 
i agree with samuelliu the last p-number in the asme code is sa-836 and refers to a forgins so i think you have to check this information


toto37
 
sandra

see asme code section IX page 65 QW 420.1 and page 101

i hope this can help
 