Apr 28, 2003 #1 sadra Petroleum Joined Jun 3, 2002 Messages 35 Location AE HI IS THERE ANY BODY CAN TELL ME WHAT IS THE P NOMBER AND GROUP NOMBER FOR A860 WPHY 65 REGARDS, R.SALIMI
HI IS THERE ANY BODY CAN TELL ME WHAT IS THE P NOMBER AND GROUP NOMBER FOR A860 WPHY 65 REGARDS, R.SALIMI
Apr 28, 2003 #2 samuelliu Mechanical Joined Jan 7, 2001 Messages 85 Location CA A860/A860M-00 is Standard Specification for Wrought High-Strength Low-Alloy Steel Butt-Welding Fittings, but there is no such ASME material existed as SA-860, so no P NOMBER AND GROUP NOMBER are available for this material. Upvote 0 Downvote
A860/A860M-00 is Standard Specification for Wrought High-Strength Low-Alloy Steel Butt-Welding Fittings, but there is no such ASME material existed as SA-860, so no P NOMBER AND GROUP NOMBER are available for this material.
May 10, 2003 #3 toto37 Industrial Joined May 8, 2003 Messages 4 Location MX i agree with samuelliu the last p-number in the asme code is sa-836 and refers to a forgins so i think you have to check this information toto37 Upvote 0 Downvote
i agree with samuelliu the last p-number in the asme code is sa-836 and refers to a forgins so i think you have to check this information toto37
May 10, 2003 #4 toto37 Industrial Joined May 8, 2003 Messages 4 Location MX sandra see asme code section IX page 65 QW 420.1 and page 101 i hope this can help Upvote 0 Downvote