Apr 28, 2008 #1 wangzh2k Mechanical Joined Dec 12, 2007 Messages 28 Location US Hi all, Is there anyone knowing the European materials vs ASTM material such as A182-316L corresponding European SS material? Thanks in advance.
Hi all, Is there anyone knowing the European materials vs ASTM material such as A182-316L corresponding European SS material? Thanks in advance.
Apr 28, 2008 #2 kalmari Mechanical Joined Dec 18, 2006 Messages 18 Location FI European standard EN 10222-5 is for stainless forging materials. This standard includes material No. 1.4404 which is similar stainless steel with low-carbon content as 316L. See websites of European material manufacturer's. Upvote 0 Downvote
European standard EN 10222-5 is for stainless forging materials. This standard includes material No. 1.4404 which is similar stainless steel with low-carbon content as 316L. See websites of European material manufacturer's.
Apr 28, 2008 Thread starter #3 wangzh2k Mechanical Joined Dec 12, 2007 Messages 28 Location US Thank you so much! Upvote 0 Downvote