Is there anyone knowing the European materials vs ASTM material such as A182-316L corresponding European SS material?

Thanks in advance.
 
European standard EN 10222-5 is for stainless forging materials. This standard includes material No. 1.4404 which is similar stainless steel with low-carbon content as 316L. See websites of European material manufacturer's.
 