Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASME SA370 Specification / material breakdown.

Status
Not open for further replies.

110277

Mechanical
Jul 18, 2003
1
Can someone provide me with the material specification and mechanical properties of ASME SA370. I work for a drilling company and need to know the hardness of this material and what it is classed as Low Carbon Steel, Alloy Steel, Construction Steel?
 
Replies continue below

Recommended for you

110277

SA370 is the standard for the mechanical testing of steel products. Tensile, bend, etc.

grayseal
 
A 370 gives various method of testing. The required values for various material are governed by the material spec. What A 370 could provide you additionally is the hardness conversion/equivalance table amongst various hardness scales.
Do you want a copy of ASTM A 370 or do you want to know the hardness limits for various materials?
 