ASME - acceptable material editions

Status
Not open for further replies.

WE.MetE

Materials
Joined
Jun 12, 2017
Messages
6
Location
US
In the 2023 Edition of ASME, Section II, Part A, Mandatory Appendix II, paragraph II-300 was completely rewritten.

For a particular material like SA-335-P91, Type 1 if ordered to a job being designed/built to the 2023 Edition of the Code, Section II, Part Table II-200-1 says that the oldest ASTM Edition is ASTM 2018. Prior to 2023, if a supplier sends in material to the 2017 edition of the code, we would accept this based on paragraph II-300 (of the 2021 Edition).

Is there some other paragraph, such as PG-10 of Section I that can be used to accept older material, older than allowed per Table II-200-1?

Thanks!
 