Is it required to list all possible filler metal options on a WPS per ASME SEC. IX? We have a number of WPSs that list only the filler used on the supporting PQR.
If a different filler is needed/requested, are we able to proceed using a filler that meets all of the ASME IX requirements even if it is not specifically listed on the WPS?