May 19, 2017 #1 Smashrc Industrial Joined May 30, 2007 Messages 1 Location HK I know this is hard coating on 7075. There are so many kind of hard coating existing. Do you know what kind is it? I see it has some texture on the coating.
I know this is hard coating on 7075. There are so many kind of hard coating existing. Do you know what kind is it? I see it has some texture on the coating.
May 20, 2017 #2 swall Materials Joined Sep 30, 2003 Messages 2,767 Location US Looks like hard coat anodize (sulfuric acid process)in the range of .001-.003" thickness. Upvote 0 Downvote