Dear Experts,

I’ve come across the procedures some paint manufacturers follow to revalidate expired coating/lining materials.


In a previous instance, we placed full responsibility on the paint manufacturer and insisted on their presence during internal inspections (both Visual and Holiday) for a Fire Water Tank. That ensured a proper accountability framework.


Now, a similar situation has come up again with the same manufacturer. They have revalidated the expired paint through our contractor, extending its validity until May 2025, although the material had already expired in January 2025. However, the material receiving inspection has not been carried out yet. The paint has been stored in a temperature-controlled (air-conditioned) facility since then.


I’d like to clarify the following:


  1. Is a third-party lab certificate for the same batch, along with a guarantee letter from the manufacturer, sufficient for acceptance?
  2. Are field tests (e.g., adhesion tests on panels) also required in this scenario?

I do have a fair understanding of how this should be handled, but would appreciate your insights or recommendations to ensure nothing is overlooked.



Thanks
 
I think it depends on the type of material, epoxy, polyurethane, polyester, etc. Is it a 1-component or 2-component coating? How long was the original shelf-life, 6 months, 1-year or 2-years? Does the manufacturer keep retention samples for each batch that they inspected? Packaging can also make a difference. How long has the manufacturer produced the product?
 
FYI... Just stumbled over this...

MIL-STD-8047 - QUALITY ASSURANCE AND SHELF-LIFE EXTENSION TESTING FOR PAINTS, SEALERS, ADHESIVES AND RELATED PRODUCTS

DOD MANUAL 4140.27, VOLUME 1 - DOD SHELF-LIFE MANAGEMENT PROGRAM: PROGRAM ADMINISTRATION
DOD MANUAL 4140.27, VOLUME 2 - DOD SHELF-LIFE MANAGEMENT PROGRAM: MATERIEL QUALITY CONTROL STORAGE STANDARDS

and for giggles... while I'm on a roll....

MIL-HDBK-695 - RUBBER PRODUCTS: RECOMMENDED SHELF LIFE

MIL-STD-3004-1 QUALITY ASSURANCE FOR BULK FUELS, LUBRICANTS, AND RELATED PRODUCTS
MIL-STD-3004-2 QUALITY ASSURANCE AND SHELF-LIFE EXTENSION TESTING FOR PACKAGED FUELS, LUBRICANTS AND RELATED PRODUCTS
 