I know this is hard coating on 7075. There are so many kind of hard coating existing. Do you know what kind is it? I see it has some texture on the coating.
 
Replies continue below

Recommended for you

Looks like hard coat anodize (sulfuric acid process)in the range of .001-.003" thickness.
 