I asked question from artificial intelligence and it saysbolt manufacturer identification markings
Put this into your search engine and you can identify the manufacture.
Thanks for your respondAI is incorrect in this case.
TS is likely Yin Shin Hardware Industry Co., Ltd, of Taiwan.
Thanks for your respond
How can you find it
Please explain
But I search TS and can't find manufacturerI followed @EdStainless' instructions exactly.
bolt manufacturer identification markings
Put this into your search engine and you can identify the manufacture.
"bolt manufacturer identification markings"
Put this into your search engine and you can identify the manufacture.
Do you check this way or only forward itToo bad.
Hi thanks for your helpManufacturer Identification Symbols - Global Fastener Platform
www.globalfastener.com