I'm looking for the welding procedure to weld stainless steel pipes diam from 10mm to 48 mm. materail AISI 316 Ti
What is the best electrode for this kind of material
Thanks
 
Suggested filler metal for joining the 316 Ti SS to 316 Ti SS is ER 316L using the GTAW process. Cleanliness is important. No preheat, and keep the interpass temperature less than 350 deg F.

Source; Avesta Welding Manual
 