Hello,

I am sure many threads might have been posted already on weldability carbon equivalent calculations. I have looked in to them but can not find what I am after.
I am looking for specific info on when one particular equation can be used, such as what type of steel and composition limits. Say for ex. Pcm say max carbon ~0.10%.
Why? I would like to not use the IIW formula for everything (in my case low alloy steel castings C-Mn-Si-Ni-Cr-Mo) and interested in the background how these were developed.
Cheers

 
Often the Material Specification or the Construction Specification will give you the formula to use. For ASTM materials it may be listed in the Supplementary requirements. If building a NACE compliant component their formula will be found within the specification. Regardless, the formula that applies should be hidden within the PO requirements, either by reference to a supplementary or to NACE or whatever spec's they dictate. It can take a good bit of time to track everything down.
 
Thank you all for the responses. Corypad, I have seen the link it is a pretty good one. Metengr, I will go through the document thanks!
jwhit, I work with the foundry and while specifying the weldability of the casting with 0.2C I ran in to trouble as CE-IIW equation gives greater values. other question I have is CE-IIW equation does not include Si in them.
 