PLease advise the compatibility of welding different material as follows:
1)ASTM A106 Gr. B
2)ASTM A333 Gr. 60
3)ASTM A333 Gr. 65
4)ASTM A105

Can these materials be welded togather?
Regards
 
A106, A333, and A105 are all CS P1 group material, and can be welded together. But, you need t verify the service condition if acceptable to mix them together.
 