Hi
I have been informed from our NDT staff that they cannot make radiography on pipe to fitting (Tee, reducers ect.) weld, if the fitting has tapered transition due to different thickness.
The explanation is that it is not possible to see root faults due to shadows.
This seem strange as both PED and ASME seem to approve tapered solution, but how can this be so if it is not possible to make NDT of the weld?
See attached picture of weld.
Hope some NDT expert can enlighten me
Thank you.
Br
Jacob