Greetings.

Could any expert recommend a method for measuring the gamma prime fraction automatically or semi-automatically, thereby avoiding manual measurement?

In my case, it is for a MarM247 superalloy blade. For example:
1750287107421.png
Reference: Khodabakhshi, A., Mashreghi, A., Shajari, Y. et al. Investigation of Microstructure Properties and Quantitative Metallography by Different Etchants in the Service-Exposed Nickel-Based Superalloy Turbine Blade. Trans Indian Inst Met 71, 849–859 (2018). https://doi.org/10.1007/s12666-017-1217-4

Thank you very much.
 
Do you have a fully automated SEM?
Everyone that I know still does electrochemical extraction and x-ray diffraction.
 
Do you have a fully automated SEM?
Everyone that I know still does electrochemical extraction and x-ray diffraction.
Thank you for your response

No, the SEM used is old. We attempted to utilize ImageJ software, but the "Threshold" function failed to accurately combine black and white, rendering it ineffective. Could you please share any effective methods you have encountered in your professional experience?

regards
 