Greetings.
Could any expert recommend a method for measuring the gamma prime fraction automatically or semi-automatically, thereby avoiding manual measurement?
In my case, it is for a MarM247 superalloy blade. For example:

Reference: Khodabakhshi, A., Mashreghi, A., Shajari, Y. et al. Investigation of Microstructure Properties and Quantitative Metallography by Different Etchants in the Service-Exposed Nickel-Based Superalloy Turbine Blade. Trans Indian Inst Met 71, 849–859 (2018). https://doi.org/10.1007/s12666-017-1217-4
Thank you very much.
Could any expert recommend a method for measuring the gamma prime fraction automatically or semi-automatically, thereby avoiding manual measurement?
In my case, it is for a MarM247 superalloy blade. For example:

Reference: Khodabakhshi, A., Mashreghi, A., Shajari, Y. et al. Investigation of Microstructure Properties and Quantitative Metallography by Different Etchants in the Service-Exposed Nickel-Based Superalloy Turbine Blade. Trans Indian Inst Met 71, 849–859 (2018). https://doi.org/10.1007/s12666-017-1217-4
Thank you very much.