Need Weld 4130 & 18-8

Status
Not open for further replies.

edmeister

Member
Joined
Jun 25, 2002
Messages
97
Location
CA
require to join 4130 rod into a 18-8 fitting. Basic strength requirement - like to avoid cracking.
Any comments & / or suggestions for filler rod. Looking at TIG process. Not a critical application - short term / corrosion susceptibility not a factor here..
 
ER309 or Nickel base alloy if PWHT is required.
 