I have taken equation for wall thickness using ASME B31.3 - PROCESS PIPING where most people are using to check WT, & not ISO 13623.
Wall thickness can be find out using ASME B31.3 (304.1.2 STRAIGHT PIPE UNDER INTERNAL PRESSURE) by following equations;
t = PD/2(SE+PY) - (3a)
t = PD/2SE - (3b)Barlaw's Formula
t = D/2(1-Sq(SE-P/SE+P) - (3c)Lame Equation
t = P(d+2c)/2[SE-P(1-Y)] - (3d)
I have taken eq.(3a) from above to calculate wall thickness.
GIVEN INPUT FROM CLIENT

Line Size = 48", Material: API 5L GR.X42, Design temp: 75 deg C, Design Press: 92 bars, Hydro test Press: 138 bars)
For calculating WT, t = PD/2(SE+PY),
Where, P = Design pressure (taken Hydro test pressure as 138 bars = 2001 psi = 2.001 ksi)
D = Pipe Outside Diameter = 48"
S = Allowable stress = 20000 = 20ksi (ASME B31.3 for API 5L X42)
E = Quality Factor = 1 (ASME B31.3)
Y = Coefficient = 0.4 (ASME B31.3)
= 2.001x48/2(20x1+2.001x0.4) = 2.308 Inches = 58.64MM
CA = 3MM
SO WT = 62MM