Very thin sheets of metal 4

Status
Not open for further replies.

vidiii

Industrial
Joined
Nov 13, 2006
Messages
36
Location
BE
Hi,

I'm working on a project where very thin metal plates are needed to obtain the optimal results. The sheets of metal must be as thin as possible.

Does somebody know a company that can deliver extremely thin sheets of metals (stainless steel, aluminium, phosphor bronze, brass). The sheets must be as thin as possible. 30um (micro meter) to 90um. (um = 1e-6m)

Until know I haven't found a company that can deliver those products, because the thickness is too small.

I sincerely hope somebody can help me. Thanks in advance.

Kindest regards,
Vidi
 
How many squre miles of each do you need?



Mike Halloran
Pembroke Pines, FL, USA
 
Thanks very much for the very valuable posts!
 
MikeHalloran: +- 1 cubic meter. It's for a project for designing a prototype.
 
For small quantities in assorted materials,
Just type foil

Al-1100 13, 15, 18, 25,51, 76 & 102 [μ]m
brass (Alloy 260) 25, 51 [μ]m
copper 25, 51, 76 & 102 [μ]m
nickel 25, 51, 76 & 102 [μ]m
stainless (304, 309 & 321) 51 [μ]m

Adhesive-backed is available, too.
 
And two more, one on each side of the pond.
(formerly known as Teledyne Rodney)

An I also recall Engineered Metals in MA, I believe that the web is
= = = = = = = = = = = = = = = = = = = =
Rust never sleeps
Neither should your protection
 