Vendors for polymer coating materials on glass

Status
Not open for further replies.

ganpule

Chemical
Jul 5, 2001
3
I am working on developing a new product which needs a barrier or protective layer coating for a high transparency optical (LCD) application. This barrier layer needs to withstand 300 C temperature for a few minutes in vacuum in a post-processing step, and 30% HCl at room temp during another post-processing step. Can somebody suggest any materials or vendors.
 