In compress,
Using slip on flange in 2" pipe sch.160 will lead to a deficiency in external fillet weld.
" UW-21: External fillet leg minimum (9.02 mm) is greater than the flange hub thickness (7.87 mm) " this message is shown during code calculation. but in UW-21 external fillet " X min = the lesser of 1.4t n or the thickness of the hub ". I think there is a problem with the software in determining the minimum requirement of External fillet leg. What do y'all think about that ?
Using slip on flange in 2" pipe sch.160 will lead to a deficiency in external fillet weld.
" UW-21: External fillet leg minimum (9.02 mm) is greater than the flange hub thickness (7.87 mm) " this message is shown during code calculation. but in UW-21 external fillet " X min = the lesser of 1.4t n or the thickness of the hub ". I think there is a problem with the software in determining the minimum requirement of External fillet leg. What do y'all think about that ?