The code now allows for UT inspection instead of RT under UW 51 (4) . If I am building a vessel and the extent of examination is outlined as UW 52 for spot RT can i substitute spot UT?
I don't see why not since it is permitted in UW-51 as an alternative to RT. You need to have a detailed map for UT as you would for spot RT. The Inspector would need to concur with this approach.
We are only certified to Div 1 so I do not have the Div 2 book to refer to. Do you know if there is a similar section in Div 1? The inspector has said as long as it is according to code he will agree but I do not have a clear answer for him. Phased array will cost more than RT for one 6" spot but again the code is not clear if that is acceptable.
Having been through several jobs using UT in lieu of RT I think you're going to find that for Spot examination, it's not worth it. Just the qualification blocks will likely cost you more than the RT you'd be doing.