Hi Guys,
Is that possible to expand (Rolling) tube to tubesheet after PWHT? The bundle is in sour services and tubesheet have both tube to tubesheet weld and grove expands area. The hardness of tube expanded area (As measured in a sample) is less than 178 Brinle after rolling.
Is that practical to perform rolling before PWHT? This will not lead to weld cracking during PWHT?
Is that possible to expand (Rolling) tube to tubesheet after PWHT? The bundle is in sour services and tubesheet have both tube to tubesheet weld and grove expands area. The hardness of tube expanded area (As measured in a sample) is less than 178 Brinle after rolling.