Hello Friends:

If I need to perform three charpy tests to cover the entire thickness range required in the project, under B 31.3. (T / 2 TO T + 6). a) These three tests should be included in the PQR that supports the single WPS. I am not sure.
b) In addition, Does the minimum thickness of the WPS will be defined as T / 2 (T smaller specimen thickness tested)?

Thaks for your help.
 
Replies continue below

Recommended for you

What are the required thicknesses for your project and then it is easier to explain and answer ?
 
Thanks Mr. DekDee:

These are the data of the material to be used in the project (under B31.3):

Material: A333 Gr 6
Thicknesses: 3/16" (5mm) to 3/4"(19mm)

Thanks



 