Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Reducing the thickness by machining to qualify for low thickness pipe WPS

Status
Not open for further replies.

infometrix

Mechanical
Joined
Oct 22, 2024
Messages
8
Location
AE
Hi everyone,
i put my case in front of welding professionals.
suppose i have a pipe 6"x15.88, APIL 5L X60.
i want welding procedure qualification for 6"x8mm.

my question is, can i reduce the thickness of 6"x15.88 to 8mm by machining till up to HAZ or little more, just to qualify for 6"x8mm because qualification of 6x15.88, i am not getting the thickness of 8mm in thickness range as per API 1104.

if it is allowed, which clause and code exactly allows the machining of high thickness to low thickness to cover or qualify for low thickness range

Thanks in adnavce.
 
Machining till HAZ? Machining should be done before welding, or am I reading your questing wrong?
 
@ kingnero (Mechanical).

machining before welding to reduce the thickness for qualification of WPS for low wall thickness. because material for low wall thickness is not available,

so my quation is, is it allowed to machine down to low wall thickness for welding procedure qualification?

thanks
 
Agree with kingnero. However, if you’re looking for a clause in the code that allows this, there isn’t one.

Just machine down your pipe to the desired thickness and record it on the PQR.

The devil is in the details; she also wears prada.
 
thank you very much. professionals
 