If you can attach a suitable ground, and immerse the rest of the part, you can measure conductance between metal and surrounding water. Debatable whether this means anything over any period of time, or in the presence of contaminants that may break down the coating...
The best way, as alluded by IRstuff, is to let the part sit outside for a year or two, and look for bubbles under the paint.