Dear Gents,


Is it allowed to tack weld with GTAW and do the final welding with SMAW process for filet welds according to ASME Codes ?

Thanks in advance
 
Replies continue below

Recommended for you

Yes, as long as you are qualified for both processes.
 
Always better to stick to a single process. Can you have a WPS that is a mix of GTAW & SMAW (not root & fill-up and final)?

DHURJATI SEN


 