No, stitch welds are intermittent welds, at fixed spaces and weld length.
As the other guys said, "tack weld " is a shop term for temporary welds to hold pieces together before making the primary weld.
Welding nuts over a clearance hole to make cheap tapped holes is good in many applications, but the weld should be defined by type, size, symbol, and whether at 2 points, 3 points or all around.