frans

Mechanical
Sep 19, 2000
41
I get more and more need to specify wear plate. Does anyone know where I can find a summary of the different kinds of wear plate available and applications, advantages/disadvantages. My application is mostly quarries, mining etc.

Thx
 
Replies continue below

Recommended for you

I am not aware of the commercial grades available. But I provide a generic classification in terms of increased wear resistance. Some of the wear plate manufacturers in their brochure furnish such data claiming their product is superior to the competition!!

low alloy steel wear plates,(with or withour surface treatment)

high manganese steel wear plates,

Ni Hard wear plates

high Cr iron wear plates


Save water Drink Beer
 
The most appropriate wear plate will vary on various factors such as on size of material, hardness, silica content, drop height ( impact ) etc. Also downtime cost / availability, and difficulty of replacement.
Item 1 in the answer above , steel wear plates, come in a multitude of grades.
Also, there are other solutions such as ceramic, and rubber/ceramic wear plates.
 