Strip Cladding
Hi experts we have a customer who requires 1.5mm SS 304L overlay on a MS pipe diameter 4 metres , thickness 18 mm and length of 5 metres . Information desired is
What will be the size of strip recommended .
What is the expected linear speed of overlay at 1.5 mm thickness .
Answers appreciated . Thanks .
Hi experts we have a customer who requires 1.5mm SS 304L overlay on a MS pipe diameter 4 metres , thickness 18 mm and length of 5 metres . Information desired is
What will be the size of strip recommended .
What is the expected linear speed of overlay at 1.5 mm thickness .
Answers appreciated . Thanks .