TugboatEng
Marine/Ocean
- Nov 1, 2015
- 11,824
Compaction of backfill that deep seems like it would take a very long time. I have seen road construction where the road bed is excavated instead of compacted and filled with lightweight cellular concrete. Perhaps they could pour the cellular concrete between sheet pile to minimize the amount of material required.