Dear sirs,
We would like to use stock tubes SA334 Gr.6 in a HE with design low temperature -46°C but in the certificate there isn't the value of impact test.
Is it mandatory to write in the certificate the values of impact test? Shall we use these tubes without any problem?
Another question, how can we know the minimum design temperature with tubes marked SA210 GrA1 (without any value of impact test)?
(OD:19,05mm thk:2,11mm)
Thank you
(sorry for my bad english)
We would like to use stock tubes SA334 Gr.6 in a HE with design low temperature -46°C but in the certificate there isn't the value of impact test.
Is it mandatory to write in the certificate the values of impact test? Shall we use these tubes without any problem?
Another question, how can we know the minimum design temperature with tubes marked SA210 GrA1 (without any value of impact test)?
(OD:19,05mm thk:2,11mm)
Thank you
(sorry for my bad english)