Hi experts,
Could you please share your experience regarding CVN impact testing for ER70S-6 filler metal?
I’m currently qualifying a PQR for A333 Gr.6 to API 5L Gr.X65 using ER70S-6 (GTAW + SMAW).
When conducting the weld metal impact test (full-size specimens) at -46 C degree, I obtained very inconsistent results: 11 J, 120 J, and 80 J.
I repeated the test on another set of CVN specimens, but the same pattern appeared — two high values and one significantly low value.
All three specimens were taken from the same area of the weld on a test coupon (pipe 6" OD, 11 mm thickness).

I’m trying to understand the cause of this variation.
Has anyone encountered this issue before? Any insights or suggestions would be greatly appreciated.

Thanks in advance!
 
There are many errors during specimen extraction, machining, and testing.
Did you witness all the steps?.
 
There are many errors during specimen extraction, machining, and testing.
Did you witness all the steps?.
No sir, we just witness the testing only.
 
And the impact test at the HAZ?

Was another test performed?
 
So you also looked at the face of the notch to assure that there was no tearing or chatter?
I am sure that no tearing or chatter at the notch.
Yesterday, I changed the CVN test to another test lab.
At the first set, results of absorbed energy are 12J, 43J, 85J.
The second set, results are 53J, 33J, 28J.
The CVN results of ER70S-6 in certficate are 151J, 153J, 147J in 1G position.
It is very difficult for me to explain the test results to Client.
 
And the impact test at the HAZ?

Was another test performed?
No sir. It is tested at weld metal.
Another test performed at other test lab. Please see my response above.
 
The consumable batch certificate is 3.1 or 2.2 ?
 
@Karik87
You said: "It is very difficult for me to explain the test results to Client."

Well, you need to read more and take a welding and NDT training course
Impact test requires a step-by-step inspection by qualified personnel.
 
Last edited:
@Karik87
You said: "It is very difficult for me to explain the test results to Client."

Well, you need to read more and take a welding and NDT training course
Impact test requires a step-by-step inspection by qualified personnel.
r6155,
Stop being so bloody critical all the time.
You do nothing on this forum but criticise.
"It is very difficult for me to explain the test results to Client." - do you with all your wisdom have an explanation to offer the Client ?
karik87 does not need to be qualified or to take a Welding or NDT training course - the test laboratories are required to be certified with qualified personnel.
He has chosen to take the samples to a 2nd laboratory and there are still issues.
Steve Jones has given a very valid response - how accurate is the consumable batch certificate ?
 
I've seen these type of results numerous times. Most often a result of notch location (weld dilution) and notch machining.
 
The consumable batch certificate is 3.1 or 2.2 ?
The consumable certificate is 3.1 with CVN results as 151J, 153J, 147J in 1G position, Sir.
 
Last edited:
I've seen these type of results numerous times. Most often a result of notch location (weld dilution) and notch machining.
This is the 1st time I have seen inconsistent results of CVN tests.
As you see the below photo, the notch location is in the middle of weld metal.
5.jpg

@SJones @DekDee @EdStainless @weldstan Thank you very much for taking the time to share your valuable opinions. Based on the discussion, I believe that the consumable batch certificate may not be fully accurate.
 
It is impossible to draw a conclusion.
 
Some of your initial post does not make sense. How are you getting full size 10x10mm charpy from a 6" x 11mm wall pipe? The curvature of the pipe would prevent that. Also, is the entire PQR pipe coupon welded with ER70S-6 GTAW? You mention you are qualifying GTAW/SMAW.

In addition to other possible causes, one reason I've seen inconsistent CVN values, is when the notch has a lot of unrefined weld metal in it. Are you doing single pass per layer, or what is your bead sequence? Bead sequences that promote grain refinement produce better and more regular CVN results. The filler metal manufacturers have that down pat, so get good and consistent results. While your filler metal certificates may demonstrate that the manufacturer can get good results with their welding technique, it doesn't mean much when the user's welding practices can be completely different.
 
How are you getting full size 10x10mm charpy from a 6" x 11mm wall pipe? The curvature of the pipe would prevent that.
You are confused, The length of the impact sample is parallel to the axis of the pipe.
 
Hah- your right on that one. For some reason I had the ASTM figure for pipe seam weld CVNs stuck in my head late at night. I think the other points are still valid though, even though my mental orientation was wrong.
 
You are comparing apples to oranges. The manufacturers data is full size all weld metal tests performed to maximize grain refinement. Yours are subsize specmens with weld metal dilution with base material with probable lesser controlled heat inputs.
 