Hi guys,

I have an issue of welding S355NL material as per AWS D1.1 code. Please help me clear it.
I have wps qualified for any group I to any group II. So can I use this wps for welding S355NL?
Thanks all.
 
No you cannot use.
The material you have listed is not recognised by AWS D.1.1 so must be qualified separately.
 
@DekDee : Thanks for your advice.
 
The Owner's representative, i.e., the Engineer, can allow a material substitution or exemption for a specific applications. As my friend DekDee says, it is not considered prequalified per AWS D1.1, so it would have to be qualified in accordance with Clause 4 of AWS D1.1.

Best regards - Al
 