May 24, 2024 #1 duongwe Mechanical Joined Jan 25, 2011 Messages 43 Location VN Dear Gents, WPS has been qualified ROOT/HOT/FILL/CAP = GTAW/GTAW/FCAW/FCAW. Now production the joint could be welded GTAW/FCAW/GTAW/FCAW or GTAW/GTAW/FCAW/GTAW? Thanks you.
Dear Gents, WPS has been qualified ROOT/HOT/FILL/CAP = GTAW/GTAW/FCAW/FCAW. Now production the joint could be welded GTAW/FCAW/GTAW/FCAW or GTAW/GTAW/FCAW/GTAW? Thanks you.
May 24, 2024 #2 david339933 Industrial Joined Jun 15, 2011 Messages 1,204 Location CA As long as the process qualified with backing has backing, no problem. Upvote 0 Downvote
May 27, 2024 #3 MUHAMMAD FAHAD RANA Materials Joined Dec 13, 2018 Messages 36 Location PK Agreed with David. I suggest, to rewrite WPS as per Actual process sequence for any query raised by client, As per code there is no issue. Fahad Upvote 0 Downvote
Agreed with David. I suggest, to rewrite WPS as per Actual process sequence for any query raised by client, As per code there is no issue. Fahad