Dear Gents,

WPS has been qualified ROOT/HOT/FILL/CAP = GTAW/GTAW/FCAW/FCAW. Now production the joint could be welded GTAW/FCAW/GTAW/FCAW or GTAW/GTAW/FCAW/GTAW?

Thanks you.
 
Replies continue below

Recommended for you

As long as the process qualified with backing has backing, no problem.
 
Agreed with David.

I suggest, to rewrite WPS as per Actual process sequence for any query raised by client, As per code there is no issue.



Fahad
 