Dear sir,
I have some question about %RT or %PT of pipe line.
Is this % of all joint for complete route line or all joint each sheet for the isometric drawing?
Example .
RT 10%
Case 1
Isometric sheet. 1) have welding joint 2 DB = RT 1 joint
Isometric sheet. 2) have welding joint 20 DB = RT 2 joint
Total RT = 3 Joint---> Correct?
If,Case 2
Isometric sheet. 1) have welding joint 2 DB = 1 joint
Isometric sheet. 2) have welding joint 2 DB = 1 joint
Total RT = 2 Joint---> Correct?
If,Case 3
If i can redesign in case 2 to one isometric drawing
I will have RT = 1 joint ----> correct?
SK.
I have some question about %RT or %PT of pipe line.
Is this % of all joint for complete route line or all joint each sheet for the isometric drawing?
Example .
RT 10%
Case 1
Isometric sheet. 1) have welding joint 2 DB = RT 1 joint
Isometric sheet. 2) have welding joint 20 DB = RT 2 joint
Total RT = 3 Joint---> Correct?
If,Case 2
Isometric sheet. 1) have welding joint 2 DB = 1 joint
Isometric sheet. 2) have welding joint 2 DB = 1 joint
Total RT = 2 Joint---> Correct?
If,Case 3
If i can redesign in case 2 to one isometric drawing
I will have RT = 1 joint ----> correct?
SK.