Husseinkhaledg

Electrical
May 27, 2020
1
w_v9h2mo.png


Where can i find the code that can tell me the required metrics for the resin used in making the casing of the circuit breakers ?

what i know.
1) IEC 60947,IEC 60898 are the codes for miniature CB and MCCB and the dont contain the information i want
2)In the section related to the casing they direct me to another Code (IEC 60695-2) which is not available for me and i believe that it talks about the method of testing of glow wire test and similar tests which is fine but what i need is after i perform the tests what are the right numbers and the right limits that the resin should succeed in
 