Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations dmapguru on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

thread712-461270: Bubble Wrap Film Plastic Resin Formulation Question

Status
Not open for further replies.

sologustavo

Materials
Joined
Jan 23, 2023
Messages
1
Location
MX
thread712-494140

I have the same problem. We have just started producing bubble wrap and we cannot find the correct formulation.

We are at 40% lldpe and 60% ldpe and many bubbles was popped. A complete row comes out deflated. I don't know if it is the mixture, because I have The lldpe has been increasing from 15% but the film came out very weak, that's why we have been increasing, but complete rows of strikeouts continue to appear, someone had the solution, I see that mah1975 you had the same problems as me now, please give me a message and tell me how you solved it, and what advice you give me in the mixes, or if someone else can help me, it will be really appreciated
 
Status