Hi All,
I have attached a micrograph of Ovako 146s case hardened steel, I am estimating around 10% RA in the case (independent lab from H/T company state "No RA") I am also achieving hardness results to support the level of RA agains independent lab results of >800Hv! Is there a more accurate way of determining without the use of XRD etc?
Thanks
I have attached a micrograph of Ovako 146s case hardened steel, I am estimating around 10% RA in the case (independent lab from H/T company state "No RA") I am also achieving hardness results to support the level of RA agains independent lab results of >800Hv! Is there a more accurate way of determining without the use of XRD etc?
Thanks