Dec 31, 2012 #1 bb29510 Geotechnical Joined Oct 3, 1999 Messages 195 Location US Can you qualify a welder on 5/16 steel plate in 1F, In d1.1? All I,m seeing is 3/8. I assume that was a minimum using table 4.11 ICC special inspector, Structural masonry, Reinforced concrete.
Can you qualify a welder on 5/16 steel plate in 1F, In d1.1? All I,m seeing is 3/8. I assume that was a minimum using table 4.11 ICC special inspector, Structural masonry, Reinforced concrete.
Jan 7, 2013 #2 Mr168 Materials Joined Aug 5, 2008 Messages 731 Location US No, unless you circumvent the requirement by going through the procedure qualification rules (see 4.19.3 in 2010 edition). Upvote 0 Downvote
No, unless you circumvent the requirement by going through the procedure qualification rules (see 4.19.3 in 2010 edition).