Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations dmapguru on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Welder Qualification with AWS A5.14 ERNiCrMo-3 according to AWS D1.1

Status
Not open for further replies.

Karik87

Mechanical
Joined
Aug 24, 2021
Messages
29
Location
VN
Hi experts,
Our company qualify welders with 6" test coupon using GTAW wire AWS A5.14 ERNiCrMo-3 and SMAW electrode AWS A5.1 ENiCrMo-3 according to AWS D1.1. Can you please advise me what the qualification range of filler metal for welders. I did not find out the clause mention to those ones.
I am appreciated for your answers.
 
In order to qualify welders using GTAW, one would need a WPS qualified by testing.

One of the essential variable for welder qualification is the F-number (of the filler metal used). AWS D1.1 doesn't list a F-number for the ENiCrMo-3. Table 6.12, item 2 really doesn't apply, but since a change in the F-number is involved, the welder would have to qualify using the ENiCrMo-3, which would have to be the same F-number as the filler metal recorded by the PQR.

Just the way I see it.

Best regards - Al
 
One must ask, why reference AWS D1.1 which is for structural steels not nonferrous materials?
 