Can you qualify a welder on 5/16 steel plate in 1F, In d1.1? All I,m seeing is 3/8. I assume that was a minimum using table 4.11

ICC special inspector, Structural masonry, Reinforced concrete.
 
Replies continue below

Recommended for you

No, unless you circumvent the requirement by going through the procedure qualification rules (see 4.19.3 in 2010 edition).
 