on the hydrotest occured leak on girth flange position.
below is detail,
D.P :10 bar
Hydrotest : 19.77bar
girth flagne : 316L, t150 X I.D900 X O.D1200 R.T.J type(with octagonal Sus gasket)
bolt : 1-1/8" Inconel 625 (bolt tighting performed 106 bar)
i'm not sure exactly why occured leak.
girth flange, gasket, bolt we already check dimension and detail. it is no problem.
could you please share experience??