If I am qualifying welders to say a WPS which requires 66 Deg C preheat for 38 mm thickness and above, and the welder qulification say is on a 38 mm plate/pipe, does the welde4r have to follow the preheat too. The reason I am asking is as per ASME section IX allows for not doing preheating/PWHT for the welder qualification test coupen even if the WPS needs so, but I could not find anything in D 1.1 Thanks and regards
Sayee Prasad R
Ph: 0097143968906
Mob: 00971507682668
Sayee Prasad R
Ph: 0097143968906
Mob: 00971507682668